Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 39.0 MPa @Strain 1.00 %, Temperature 200 °C |
5660 psi @Strain 1.00 %, Temperature 392 °F |
|
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off.. |
|||
Tensile Stress | 39.0 MPa @Strain 10.0 %, Temperature 23.0 °C |
5660 psi @Strain 10.0 %, Temperature 73.4 °F |
|
Solvay TECHNYL® A 205F PA66, Conditioned Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Stress | 39.0 MPa @Strain 20.0 %, Temperature 80.0 °C |
5660 psi @Strain 20.0 %, Temperature 176 °F |
|
Solvay TECHNYL® A 205F PA66, DRY Description: TECHNYL ® A 205F is an unreinforced polyamide 66 for injection molding. It is available in natural color.Benefits: The product offers two main advantages: excellent filling qualities.. |
|||
Tensile Stress | 39.0 MPa @Strain 8.00 %, Temperature 30.0 °C |
5660 psi @Strain 8.00 %, Temperature 86.0 °F |
ISO 527 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |