Mechanical Properties Metric English Comments
Tensile Stress 3.90 MPa

@Strain 100 %
566 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S KA 80A-3S1770 Thermoplastic Elastomer (TPE)
OnFlex™-S KA thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p..
Tensile Stress 3.90 MPa

@Strain 300 %
566 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S KE 50A-3S1731 Thermoplastic Elastomer (TPE)
OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p..
Tensile Stress 3.90 MPa

@Strain 100 %,
Temperature 23.0 °C
566 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7680-1 (Natural) Thermoplastic Elastomer (TPE)
Dynaflex™ G7680-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polyprop..
Tensile Stress 3.90 MPa

@Strain 100 %,
Temperature 23.0 °C
566 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7680-9 (Black) Thermoplastic Elastomer (TPE)
Dynaflex™ G7680-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl..
Tensile Stress 3.90 MPa

@Strain 10.0 %
566 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® EM400-BP TPC-ET
34 Shore D, Injection Molding or Extrusion Grade
Tensile Stress 3.90 MPa

@Strain 5.68 %,
Temperature 90.0 °C
566 psi

@Strain 5.68 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT  (Unverified Data**)
Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl..
Tensile Stress 3.90 MPa

@Strain 0.0700 %,
Temperature 150 °C
566 psi

@Strain 0.0700 %,
Temperature 302 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6  (Unverified Data**)
Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc..
Copyright © lookpolymers.com All Rights Reserved