Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.52 MPa @Strain 300 %, Temperature 23.0 °C |
511 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versalloy™ HC 9210-70N Thermoplastic Elastomer (TPE) Versalloy™ HC 9210-70N is a USP Class VI, TPV alloy targeted for injection molding healthcare applications such as disposable medical items and soft-touch overmolding for surgical grips. Product ex.. |
|||
Tensile Stress | 3.52 MPa @Strain 300 % |
511 psi @Strain 300 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ EG-9072 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun.. |
|||
Tensile Stress | 3.52 MPa @Strain 200 % |
511 psi @Strain 200 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ EG-9165 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Tensile Stress | 3.52 MPa @Strain 86.68 %, Temperature 100 °C |
511 psi @Strain 86.68 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.52 MPa @Strain 3.88 %, Temperature 90.0 °C |
511 psi @Strain 3.88 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.52 MPa @Strain 0.150 %, Temperature 23.0 °C |
511 psi @Strain 0.150 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien.. |
|||
Tensile Stress | 3.52 MPa @Strain 27.31 %, Temperature 90.0 °C |
511 psi @Strain 27.31 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.52 MPa @Strain 16.75 %, Temperature 60.0 °C |
511 psi @Strain 16.75 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.52 MPa @Strain 21.33 %, Temperature 180 °C |
511 psi @Strain 21.33 %, Temperature 356 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |