Mechanical Properties Metric English Comments
Tensile Stress 3.38 MPa

@Strain 100 %
490 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® C4970 TPE, Transparent
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf..
Tensile Stress 3.38 MPa

@Strain 300 %
490 psi

@Strain 300 %
NEU NeuSoft™ 602-60A Ester TPU / SBC blend
Tensile Stress 3.38 MPa

@Strain 100 %,
Temperature 23.0 °C
490 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G2701-1000-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G2701-1000-02 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Adhesion to Polypropylene - Excellent Colorability - Good ..
Tensile Stress 3.38 MPa

@Strain 300 %
490 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ XL-2065 Thermoplastic Polyolefin Elastomer (TPO (POE))
PolyOne's Elastamax™ XL thermoplastic olefins (TPOs) are based on pelletized blends of polyolefin resins and select elastomers such EPDM. These materials have been engineered to provide a balance o..
Tensile Stress 3.38 MPa

@Strain 63.38 %,
Temperature 100 °C
490 psi

@Strain 63.38 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 3.38 MPa

@Strain 0.0600 %,
Temperature 150 °C
490 psi

@Strain 0.0600 %,
Temperature 302 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)  (Unverified Data**)
Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed ..
Tensile Stress 3.38 MPa

@Strain 0.200 %,
Temperature -20.0 °C
490 psi

@Strain 0.200 %,
Temperature -4.00 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010  (Unverified Data**)
Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s..
Tensile Stress 3.38 MPa

@Strain 120.08 %,
Temperature 120 °C
490 psi

@Strain 120.08 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers
Tensile Stress 3.38 MPa

@Strain 72.42 %,
Temperature 120 °C
490 psi

@Strain 72.42 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process..