Mechanical Properties Metric English Comments
Tensile Stress 3.22 MPa

@Strain 42.0 %,
Temperature 90.0 °C
467 psi

@Strain 42.0 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 3.22 MPa

@Strain 85.58 %,
Temperature 120 °C
467 psi

@Strain 85.58 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 3.22 MPa

@Strain 58.08 %,
Temperature 120 °C
467 psi

@Strain 58.08 %,
Temperature 248 °F
ISO 527
DuPont Performance Polymers Hytrel® G4078W TPC-ET  (Unverified Data**)
Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject..