Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.21 MPa @Strain 40.77 %, Temperature 100 °C |
466 psi @Strain 40.77 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |