Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.08 MPa @Strain 100 % |
447 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® F02-087A TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |
|||
Tensile Stress | 3.08 MPa @Strain 300 % |
447 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P2945T TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 3.08 MPa @Strain 31.86 %, Temperature 100 °C |
447 psi @Strain 31.86 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.08 MPa @Strain 46.89 %, Temperature 60.0 °C |
447 psi @Strain 46.89 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |