Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.00 MPa @Strain 100 % |
435 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S HF 80A-3S1986 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tensile Stress | 3.00 MPa @Strain 100 % |
435 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S KE 70A-3S1726 Thermoplastic Elastomer (TPE) OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p.. |
|||
Tensile Stress | 3.00 MPa @Strain 100 % |
435 psi @Strain 100 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ EG-9165 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Tensile Stress | 3.00 MPa @Strain 100 %, Temperature 23.0 °C |
435 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynalloy™ OBC 8100-N65 Thermoplastic Elastomer (TPE) Dynalloy™ OBC8100-N65 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t.. |
|||
Tensile Stress | 3.00 MPa @Strain 100 % |
435 psi @Strain 100 % |
Average; ASTM D412 Method A |
Seals Eastern 5753 Fluorocarbon-Elastomer Features:MIL-SpecFKM general serviceInformation provided by Seals Eastern. |
|||
Tensile Stress | 3.00 MPa @Strain 0.0960 %, Time 3600 sec |
435 psi @Strain 0.0960 %, Time 1.00 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica.. |
|||
Tensile Stress | 3.00 MPa @Strain 0.103 %, Time 36000 sec |
435 psi @Strain 0.103 %, Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica.. |
|||
Tensile Stress | 3.00 MPa @Strain 0.111 %, Time 360000 sec |
435 psi @Strain 0.111 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica.. |
|||
Tensile Stress | 3.00 MPa @Strain 0.121 %, Time 3.60e+6 sec |
435 psi @Strain 0.121 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica.. |
|||
Tensile Stress | 3.00 MPa @Strain 0.130 %, Time 3.60e+7 sec |
435 psi @Strain 0.130 %, Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G14A NC010A Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Polyamide 66 Zytel 80G14A NC010A is a 14% glass fiber reinforced toughened high flow polyamide 66 resin. It offers outstanding performance in injection molding applica.. |
|||
Tensile Stress | 3.00 MPa @Strain 10.0 % |
435 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® XG5855 TPC-ET Extrusion Grade |
|||
Tensile Stress | 3.00 MPa @Strain 5.00 %, Temperature 23.0 °C |
435 psi @Strain 5.00 %, Temperature 73.4 °F |
ASTM D638 |
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**) Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject.. |
|||
Tensile Stress | 3.00 MPa @Strain 0.165 %, Time 36000 sec |
435 psi @Strain 0.165 %, Time 10.0 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Stress | 3.00 MPa @Strain 0.192 %, Time 360000 sec |
435 psi @Strain 0.192 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Stress | 3.00 MPa @Strain 0.231 %, Time 3.60e+6 sec |
435 psi @Strain 0.231 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Stress | 3.00 MPa @Strain 0.146 %, Time 3600 sec |
435 psi @Strain 0.146 %, Time 1.00 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Stress | 3.00 MPa @Strain 0.297 %, Time 3.60e+7 sec |
435 psi @Strain 0.297 %, Time 10000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Stress | 3.00 MPa @Strain 300 % |
435 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G55A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G55A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 3.00 MPa @Strain 100 % |
435 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 7070A Thermoplastic Polyurethane Elastomer Zythane™ 7070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | >= 3.00 MPa @Strain 300 % |
>= 435 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 265A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Stress | >= 3.00 MPa @Strain 100 % |
>= 435 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 465A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | 3.00 MPa @Strain 300 % |
435 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ G55A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G55A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |