Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.87 MPa @Strain 0.200 %, Temperature 80.0 °C |
416 psi @Strain 0.200 %, Temperature 176 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D.. |
|||
Tensile Stress | 2.87 MPa @Strain 0.0600 %, Temperature 180 °C |
416 psi @Strain 0.0600 %, Temperature 356 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)
(Unverified Data**) Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed .. |
|||
Tensile Stress | 2.87 MPa @Strain 0.130 %, Temperature -40.0 °C |
416 psi @Strain 0.130 %, Temperature -40.0 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010
(Unverified Data**) Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s.. |
|||
Tensile Stress | 2.87 MPa @Strain 0.720 %, Temperature 90.0 °C |
416 psi @Strain 0.720 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien.. |
|||
Tensile Stress | 2.87 MPa @Strain 37.16 %, Temperature 60.0 °C |
416 psi @Strain 37.16 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.87 MPa @Strain 187.85 %, Temperature 90.0 °C |
416 psi @Strain 187.85 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |