Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 27.0 MPa @Strain 6.00 %, Temperature 60.0 °C |
3920 psi @Strain 6.00 %, Temperature 140 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 27.0 MPa @Strain 100 %, Temperature 80.0 °C |
3920 psi @Strain 100 %, Temperature 176 °F |
|
Solvay TECHNYL® eXten D 437P PA6.10 Description: TECHNYL® eXten D 437P is a high viscosity, unfilled, plasticized, UV and heat stabilized PA6.10 for extrusion applications. Technyl® eXten D 437P is a partially biosourced materia.. |
|||
Tensile Stress | 27.0 MPa @Strain 4.20 %, Temperature 90.0 °C |
3920 psi @Strain 4.20 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Tensile Stress | 27.0 MPa @Strain 0.250 %, Temperature 23.0 °C |
3920 psi @Strain 0.250 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Polyethylene Terephthalate Rynite 530 NC010 is a 30% glass fiber reinforced modified polyethylene terephthalate resin with an outstanding balance of strength stiffness and tough.. |
|||
Tensile Stress | 27.0 MPa @Strain 0.520 %, Temperature 150 °C |
3920 psi @Strain 0.520 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL NC010 Polyphthalamide (PPA) Zytel® HTN52G35HSL NC010 is a 35% glass reinforced, heat stabilized, lubricated high performance polyamide resin that can be molded in water heated molds.Information provided by DuPont Performance .. |
|||
Tensile Stress | 27.0 MPa @Strain 0.500 %, Temperature 100 °C |
3920 psi @Strain 0.500 %, Temperature 212 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G20NH BK337 Polyphthalamide (PPA) Zytel® HTNFR52G20NH BK337 is a 20% glass reinforced, flame retardant, lubricated high performance polyamide resin. It is also a PPA resin and it uses a non-halogenated flame retardant.Information p.. |
|||
Tensile Stress | 27.0 MPa @Strain 50.0 % |
3920 psi @Strain 50.0 % |
50%RH; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010 Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced.. |
|||
Tensile Stress | 27.0 MPa @Strain 300 % |
3920 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 4060D Thermoplastic Polyurethane Elastomer Zythane™ 4060D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 27.0 MPa @Strain 300 % |
3920 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 6050D Thermoplastic Polyurethane Elastomer Zythane™ 6050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 27.0 MPa @Strain 300 % |
3920 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 7050D Thermoplastic Polyurethane Elastomer Zythane™ 7050D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 27.0 MPa @Strain 1.00 %, Temperature 23.0 °C |
3920 psi @Strain 1.00 %, Temperature 73.4 °F |
ISO 527 |
BASF Ultrason S 3010 PSU Ultrason S 3010 is an unreinforced, higher viscosity injection molding and extrusion PSU grade, tougher and with improved chemical resistance. It conforms to FDA requirements of 21 CFR 177.1655. |
|||
Tensile Stress | 27.0 MPa @Strain 50.0 %, Temperature 120 °C |
3920 psi @Strain 50.0 %, Temperature 248 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |
|||
Tensile Stress | 27.0 MPa @Strain 50.0 %, Temperature 150 °C |
3920 psi @Strain 50.0 %, Temperature 302 °F |
DAM; ISO 527 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |