Mechanical Properties Metric English Comments
Tensile Stress 26.86 MPa

@Strain 1.18 %,
Temperature -40.0 °C
3896 psi

@Strain 1.18 %,
Temperature -40.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610  (Unverified Data**)
Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien..
Tensile Stress 26.86 MPa

@Strain 23.59 %,
Temperature 90.0 °C
3896 psi

@Strain 23.59 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 153HSL NC010 Nylon 612  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 612 Information provided by DuPont Performance Polymers