Tensile Stress 250 MPa

@Strain 2.00 %,
Temperature 0.000 °C
36300 psi

@Strain 2.00 %,
Temperature 32.0 °F
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Tensile Stress 250 MPa

@Diameter 25.0 - 50.0 mm,
Strain 0.200 %
36300 psi

@Diameter 0.984 - 1.97 in,
Strain 0.200 %
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..
Tensile Stress 250 MPa

@Diameter 55.0 - 100 mm,
Strain 0.200 %
36300 psi

@Diameter 2.17 - 3.94 in,
Strain 0.200 %
United Cast Bar Unibar 400-15 As Cast Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..
Tensile Stress 250 MPa

@Diameter 25.0 - 50.0 mm,
Strain 0.200 %
36300 psi

@Diameter 0.984 - 1.97 in,
Strain 0.200 %
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..
Tensile Stress 250 MPa

@Diameter 55.0 - 100 mm,
Strain 0.200 %
36300 psi

@Diameter 2.17 - 3.94 in,
Strain 0.200 %
United Cast Bar Unibar 400-15 Fully Annealed Continuously Cast Spheroidal Graphite Iron
Offers superior machinability combined with good impact, fatigue, electrical conductivity and magnetic permeability. Noise and vibration damping are good in this grade.Unibar 400-15 is not recommend..