Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.48 MPa @Strain 300 %, Temperature 23.0 °C |
360 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ CL2250 Thermoplastic Elastomer (TPE) Versaflex™ CL2250 is an easy processing compound designed for use in injection molding applications where FDA compliance, clarity and enhanced heat resistance are required. - Excellent Clarity - Ov.. |
|||
Tensile Stress | 2.48 MPa @Strain 100 %, Temperature 21.0 °C |
360 psi @Strain 100 %, Temperature 69.8 °F |
Die C2 hr; ASTM D412 |
PolyOne Versalloy™ XL 9070-1 Thermoplastic Elastomer (TPE) Versalloy™ XL 9070-1 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Excellent Flow for Long, Thin Flow Paths - Exceptional Colorability - Ov.. |
|||
Tensile Stress | 2.48 MPa @Strain 100 %, Temperature 23.0 °C |
360 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versalloy™ XL 9070X-9 Thermoplastic Elastomer (TPE) Versalloy™ XL 9070X-9 is a TPV alloy with exceptional flow properties and surface aesthetics for a variety of applications. - Exceptional Flow for Long, Thin Flow Paths - Overmold Adhesion to Polyp.. |
|||
Tensile Stress | 2.48 MPa @Strain 100 %, Temperature 23.0 °C |
360 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7430-9001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7430-9001-00 is an easy processing, high performance compound designed for use in applications requiring tough, durable material. - Excellent Heat Stability - Good Ozone and UV Stability.. |
|||
Tensile Stress | 2.48 MPa @Strain 300 %, Temperature 23.0 °C |
360 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7640-9 (Black) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-9 (Black) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropyl.. |
|||
Tensile Stress | 2.48 MPa @Strain 300 %, Temperature 23.0 °C |
360 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7950-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tensile Stress | 2.48 MPa @Strain 300 %, Temperature 23.0 °C |
360 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1001-00 is an easy processing, general purpose material designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypro.. |
|||
Tensile Stress | 2.48 MPa @Strain 300 %, Temperature 23.0 °C |
360 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7950-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7950-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tensile Stress | 2.48 MPa @Strain 300 %, Temperature 23.0 °C |
360 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7950-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7950-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Tensile Stress | 2.48 MPa @Strain 300 %, Temperature 23.0 °C |
360 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G7640-1 (Natural) Thermoplastic Elastomer (TPE) Dynaflex™ G7640-1 (Natural) is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Non-Slip Grip - Overmold Adhe.. |
|||
Tensile Stress | >= 2.48 MPa @Strain 50.0 % |
>= 360 psi @Strain 50.0 % |
ASTM D412 Method A |
Seals Eastern 5794 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |