Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 24.29 MPa @Strain 0.690557 %, Temperature 140 °C |
3522 psi @Strain 0.690557 %, Temperature 284 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |