Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 18.0 MPa @Strain 50.0 % |
2610 psi @Strain 50.0 % |
conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 3982 PA12 Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good ch.. |
|||
Tensile Stress | 18.0 MPa @Strain 50.0 % |
2610 psi @Strain 50.0 % |
dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 3982 PA12 Product description: Grilamid XE 3982 is a highly flexible extrusion grade, based on Polyamide 12 with following main attributes: High flexibilityLow plasticizer migration (low blooming)Very good ch.. |
|||
Tensile Stress | 18.0 MPa @Strain 300 % |
2610 psi @Strain 300 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |
|||
Tensile Stress | 18.0 MPa @Strain 0.440 %, Temperature 150 °C |
2610 psi @Strain 0.440 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSLX BK357 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSLX BK357 is a 35% glass fiber reinforced heat stabilized black polyamide 66 for injection molding.Information provided by DuPont Perfor.. |
|||
Tensile Stress | 18.0 MPa @Strain 0.150 %, Temperature -40.0 °C |
2610 psi @Strain 0.150 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30NH BK337 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It.. |
|||
Tensile Stress | 18.0 MPa @Strain 0.480 %, Temperature 23.0 °C |
2610 psi @Strain 0.480 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 135F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 135F NC010 is a nucleated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont Pe.. |
|||
Tensile Stress | 18.0 MPa @Strain 300 % |
2610 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 6070A Thermoplastic Polyurethane Elastomer Zythane™ 6070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 18.0 MPa @Strain 200 % |
2610 psi @Strain 200 % |
|
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Tensile Stress | 18.0 MPa @Strain 300 % |
2610 psi @Strain 300 % |
|
AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Tensile Stress | 18.0 MPa @Strain 200 % |
2610 psi @Strain 200 % |
|
AorTech Biomaterials Elast-Eon™ E2-852 Biomedical Polyurethane Pellets Elast-Eon™ 2-852 is a polyurethane with a 52% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DM.. |
|||
Tensile Stress | 18.0 MPa @Strain 300 % |
2610 psi @Strain 300 % |
|
AorTech Biomaterials Elast-Eon™ E2-945 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Tensile Stress | >= 18.0 MPa @Strain 300 % |
>= 2610 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 490A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | >= 18.0 MPa @Strain 100 % |
>= 2610 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 498A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | >= 18.0 MPa @Strain 100 % |
>= 2610 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 664D Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | 18.0 MPa @Strain 10.0 %, Time 3.60e+6 sec |
2610 psi @Strain 10.0 %, Time 1000 hour |
60°C; ISO 527 |
BASF Ultradur B 4520 PBT Ultradur B4520 is a medium viscosity, rapidly freezing injection molding grade. |