Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 13.97 MPa @Strain 8.87 %, Temperature 90.0 °C |
2026 psi @Strain 8.87 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3261TL NC010 Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261TL NC010 is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient by.. |