Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 13.2 MPa @Strain 0.250 %, Temperature -20.0 °C |
1910 psi @Strain 0.250 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 13.2 MPa @Strain 3.20 %, Temperature 160 °C |
1910 psi @Strain 3.20 %, Temperature 320 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. .. |