Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 12.95 MPa @Strain 47.26 %, Temperature 100 °C |
1878 psi @Strain 47.26 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |