Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 12.5 MPa @Strain 100 % |
1810 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Telcar® TL-88-N809C Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Stress | 12.5 MPa @Strain 50.0 % |
1810 psi @Strain 50.0 % |
ISO 527-1/-2 |
DSM Arnitel® VT3108 TPC-ET Extrusion Grade, High Breathable, Drying of Material Required |
|||
Tensile Stress | 12.5 MPa @Strain 10.9 %, Temperature 90.0 °C |
1810 psi @Strain 10.9 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.5 MPa @Strain 10.9 %, Temperature 90.0 °C |
1810 psi @Strain 10.9 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe.. |
|||
Tensile Stress | 12.5 MPa @Strain 50.0 % |
1810 psi @Strain 50.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® DYM250S BK472 TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsHytrel DYM250S BK472 is a medium modulus resin suited for injection molding of Air Bag Depl.. |
|||
Tensile Stress | 12.5 MPa @Strain 0.800 %, Temperature 150 °C |
1810 psi @Strain 0.800 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 12.5 MPa @Strain 0.830 %, Temperature 90.0 °C |
1810 psi @Strain 0.830 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |
|||
Tensile Stress | 12.48 MPa @Strain 0.240 %, Temperature 90.0 °C |
1810 psi @Strain 0.240 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE350064 BK544 Polyphthalamide (PPA)
(Unverified Data**) Carbon Fiber Reinforced Toughened PPA High Performance Polyamide Zytel HTNFE350064 BK544 is a carbon fiber reinforced toughened heat stabilized conductive high performance polyamide resin developed .. |
|||
Tensile Stress | 12.48 MPa @Strain 100.05 %, Temperature 150 °C |
1810 psi @Strain 100.05 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010 UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight... |
|||
Tensile Stress | 12.5 MPa @Strain 0.250 %, Temperature 23.0 °C |
1810 psi @Strain 0.250 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |