Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 11.78 MPa @Strain 98.78 %, Temperature 120 °C |
1709 psi @Strain 98.78 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 11.78 MPa @Strain 43.21 %, Temperature 90.0 °C |
1709 psi @Strain 43.21 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC4601 NC010 Nylon
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide Developed for Extrusion Zytel RS LC4601 NC010 is a flexible toughened and plasticized polyamide resin intended for extrusion applications.Informatio.. |