Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 11.65 MPa @Strain 85.29 %, Temperature 120 °C |
1690 psi @Strain 85.29 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 11.65 MPa @Strain 0.230 %, Temperature 150 °C |
1690 psi @Strain 0.230 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 77G43L NC010 Nylon 612
(Unverified Data**) 43% Glass Reinforced Polyamide 612Zytel 77G43L NC010 is a 43% glass fiber reinforced polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |