Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 11.29 MPa @Strain 46.41 %, Temperature 120 °C |
1637 psi @Strain 46.41 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |