Polymer Property : Tensile Stress = 1617 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 11.15 MPa

@Strain 36.1 %,
Temperature 120 °C
1617 psi

@Strain 36.1 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers
Tensile Stress 11.15 MPa

@Strain 0.210 %,
Temperature 180 °C
1617 psi

@Strain 0.210 %,
Temperature 356 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)  (Unverified Data**)
35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e..