Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 90.66 MPa @Strain 0.990 %, Temperature 40.0 °C |
13150 psi @Strain 0.990 %, Temperature 104 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66
(Unverified Data**) Zytel® 70G35HSLRA4 BK267 is a 35% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding. It has excellent flow characteristics.Information provided .. |
|||
Tensile Stress | 90.66 MPa @Strain 1.42 %, Temperature 40.0 °C |
13150 psi @Strain 1.42 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5329 BK503 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene TerephthalateInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 90.65 MPa @Strain 0.980 %, Temperature 0.000 °C |
13150 psi @Strain 0.980 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin.. |
|||
Tensile Stress | 90.68 MPa @Strain 1.99 %, Temperature -20.0 °C |
13150 psi @Strain 1.99 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6
(Unverified Data**) 15% Glass Reinforced Heat Stabilized Polyamide 6 Zytel BM73G15THS is a 15% glass fiber reinforced heat stabilized lubricated toughened polyamide 6 for blow molding.Information provided by DuPont Per.. |
|||
Tensile Stress | 90.68 MPa @Strain 1.00 %, Temperature 40.0 °C |
13150 psi @Strain 1.00 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 52G35HSL BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide Zytel HTN52G35HSL BK083 is a 35% glass reinforced heat stabilized lubricated high performance polyamide resin that can be molded in water heated m.. |