Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.50 MPa @Strain 100 % |
1230 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ V 3050D-S0097 Thermoplastic Elastomer (TPE) OnFlex™-V provides the performance of traditional vulcanised rubber, but with the processability of a thermoplastic. OnFlex™-V 3000 series thermoplastic elastomer compounds are based on a polyolef.. |
|||
Tensile Stress | 8.51 MPa @Strain 300 %, Temperature 23.0 °C |
1230 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ CL E90 Thermoplastic Elastomer (TPE) Versaflex™ CL E90 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E90 is also formulated without the use of plasticizer.. |
|||
Tensile Stress | 8.48 MPa @Strain 100 % |
1230 psi @Strain 100 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ EG-9190 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Tensile Stress | 8.48 MPa @Strain 100 % |
1230 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Telcar® TL-340-S Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tensile Stress | 8.50 MPa @Strain 1.60 %, Temperature 90.0 °C |
1230 psi @Strain 1.60 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.47 MPa @Strain 174.29 %, Temperature 90.0 °C |
1230 psi @Strain 174.29 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.50 MPa @Strain 249.44 %, Temperature 120 °C |
1230 psi @Strain 249.44 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.45 MPa @Strain 23.65 %, Temperature 90.0 °C |
1230 psi @Strain 23.65 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.47 MPa @Strain 71.79 %, Temperature 100 °C |
1230 psi @Strain 71.79 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.47 MPa @Strain 60.24 %, Temperature 120 °C |
1230 psi @Strain 60.24 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.45 MPa @Strain 108.54 %, Temperature 100 °C |
1230 psi @Strain 108.54 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.50 MPa @Strain 5.00 %, Temperature 23.0 °C |
1230 psi @Strain 5.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.47 MPa @Strain 0.230 %, Temperature 150 °C |
1230 psi @Strain 0.230 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin.. |
|||
Tensile Stress | 8.48 MPa @Strain 0.100 %, Temperature 150 °C |
1230 psi @Strain 0.100 %, Temperature 302 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon
(Unverified Data**) Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve.. |
|||
Tensile Stress | 8.51 MPa @Strain 35.0 %, Temperature 100 °C |
1230 psi @Strain 35.0 %, Temperature 212 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Tensile Stress | 8.50 MPa @Strain 50.0 % |
1230 psi @Strain 50.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® G4078 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.45 MPa @Strain 6.00 %, Temperature 23.0 °C |
1230 psi @Strain 6.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G5544 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G5544 is a medium modulus grade with nominal hardness of 55D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 8.50 - 11.5 MPa @Strain 200 % |
1230 - 1670 psi @Strain 200 % |
TM-019G |
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc... |
|||
Tensile Stress | 8.50 - 11.5 MPa @Strain 200 % |
1230 - 1670 psi @Strain 200 % |
TM-019G |
AorTech Biomaterials Elast-Eon™ E2A Biomedical Polyurethane Pellets Elast-Eon™ 2A is a polyurethane with a 40% hard segment content and a mixed polyether/siloxane soft segment. It comes in pellet form. The pellets are colorless to yellowish and are soluble in DMAc... |
|||
Tensile Stress | >= 8.50 MPa @Strain 100 % |
>= 1230 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 290A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance and transparency which can meet different demands in various industryInformation from Dawnentech |
|||
Tensile Stress | >= 8.50 MPa @Strain 300 % |
>= 1230 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 682A Polyester and Polyether based TPU Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |