Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.86 MPa @Strain 300 %, Temperature 23.0 °C |
1140 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2780-0001 Thermoplastic Elastomer (TPE) Dynaflex™ G2780-0001 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmo.. |
|||
Tensile Stress | 7.86 MPa @Strain 300 %, Temperature 23.0 °C |
1140 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Dynaflex™ G2780C Thermoplastic Elastomer (TPE) Dynaflex™ G2780C is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Excellent Colorability - Good Ozone and UV Stability - Overmold A.. |
|||
Tensile Stress | 7.89 MPa @Strain 33.37 %, Temperature 40.0 °C |
1140 psi @Strain 33.37 %, Temperature 104 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.89 MPa @Strain 153.83 %, Temperature 90.0 °C |
1140 psi @Strain 153.83 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.88 MPa @Strain 37.39 %, Temperature 100 °C |
1140 psi @Strain 37.39 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5553FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.85 MPa @Strain 4.57 %, Temperature 23.0 °C |
1140 psi @Strain 4.57 %, Temperature 73.4 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.88 MPa @Strain 37.39 %, Temperature 100 °C |
1140 psi @Strain 37.39 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5556 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.84 MPa @Strain 173.61 %, Temperature 120 °C |
1140 psi @Strain 173.61 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 7.83 MPa @Strain 103.46 %, Temperature 150 °C |
1140 psi @Strain 103.46 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.83 MPa @Strain 142.91 %, Temperature 120 °C |
1140 psi @Strain 142.91 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.86 MPa @Strain 174.81 %, Temperature 120 °C |
1140 psi @Strain 174.81 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.87 MPa @Strain 24.3 %, Temperature 40.0 °C |
1140 psi @Strain 24.3 %, Temperature 104 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET