Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 75.6 MPa @Strain 1.05 %, Temperature 40.0 °C |
11000 psi @Strain 1.05 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal.. |
|||
Tensile Stress | 76.1 MPa @Strain 15.4 %, Temperature 0.000 °C |
11000 psi @Strain 15.4 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Tensile Stress | 75.5 MPa @Strain 9.30 %, Temperature 0.000 °C |
11000 psi @Strain 9.30 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG500P is a medium viscosity acetal homopolymer with improved thermal stability. It has been developed for consider.. |
|||
Tensile Stress | 75.5 MPa @Strain 0.420 %, Temperature -40.0 °C |
11000 psi @Strain 0.420 %, Temperature -40.0 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Tensile Stress | 75.9 MPa @Strain 0.470 %, Temperature 0.000 °C |
11000 psi @Strain 0.470 %, Temperature 32.0 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Tensile Stress | 75.8 MPa @Strain 4.27 %, Temperature 150 °C |
11000 psi @Strain 4.27 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G35HSLRA4 BK267 is a 35% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection m.. |
|||
Tensile Stress | 75.85 MPa @Strain 5.90 %, Temperature 23.0 °C |
11000 psi @Strain 5.90 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |
|||
Tensile Stress | 75.6 MPa @Strain 3.40 %, Temperature 90.0 °C |
11000 psi @Strain 3.40 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |
|||
Tensile Stress | 75.8 MPa @Strain 0.0500 % |
11000 psi @Strain 0.0500 % |
Process Temperature T4 |
COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S300 - Sylramic SiC Preceramic Polymer Matrix Precursors: S300 - .. |
|||
Tensile Stress | 75.8 MPa @Strain 0.0500 % |
11000 psi @Strain 0.0500 % |
Process Temperature T1 |
COI Ceramics Sylramic™ S300 Silicon Carbide Ceramic Matrix Composite, SiC Description: Engineered ceramic composite structures for a broad range of industries and applications.Reinforcing Fiber Flexibility: S300 - Sylramic SiC Preceramic Polymer Matrix Precursors: S300 - .. |
|||
Tensile Stress | 75.6 MPa @Strain 1.84 %, Temperature 90.0 °C |
11000 psi @Strain 1.84 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 545 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 45% Glass Reinforced Polyethylene Terephthalate Rynite 545 NC010 is a 45% glass reinforced modified polyethylene terephthalate with greater strength and stiffness excellent dimensional stability and.. |