Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 0.0800 MPa @Strain 300 % |
11.6 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® C49C15 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 0.0800 MPa @Strain 100 % |
11.6 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® C4902 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 0.0800 MPa @Strain 300 % |
11.6 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® C49C10 TPE, Transparent Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsSporting GoodsWire & Cable ElectronicsMedical DevicesPlastic TougheningInf.. |
|||
Tensile Stress | 0.0800 MPa @Strain 0.0300 %, Temperature -40.0 °C |
11.6 psi @Strain 0.0300 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 3061HSL BK039A Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3061HSL BK039A is a renewably sourced polyamide 610 resin containing a minimum of 60% renewably sourced ingredie.. |
|||
Tensile Stress | 0.0800 MPa @Strain 0.000 %, Temperature 60.0 °C |
11.6 psi @Strain 0.000 %, Temperature 140 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010
(Unverified Data**) Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s.. |
|||
Tensile Stress | 0.0800 MPa @Strain 0.000 %, Temperature 90.0 °C |
11.6 psi @Strain 0.000 %, Temperature 194 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010
(Unverified Data**) Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s.. |
|||
Tensile Stress | 0.0800 MPa @Strain 0.000 %, Temperature 90.0 °C |
11.6 psi @Strain 0.000 %, Temperature 194 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® RS LC1600 BK385 Nylon 1010
(Unverified Data**) Zytel® RS LC1600 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced ingredient by weight. It is flexible, toughened, plasticized, UV and heat stabilized and s.. |