Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 72.59 MPa @Strain 2.90 %, Temperature 150 °C |
10530 psi @Strain 2.90 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo.. |
|||
Tensile Stress | 72.58 MPa @Strain 2.82 %, Temperature 40.0 °C |
10530 psi @Strain 2.82 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® BM73G15THS BK317 Nylon 6
(Unverified Data**) 15% Glass Reinforced Heat Stabilized Polyamide 6 Zytel BM73G15THS is a 15% glass fiber reinforced heat stabilized lubricated toughened polyamide 6 for blow molding.Information provided by DuPont Per.. |