Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 93.47 MPa @Strain 0.820 %, Temperature -20.0 °C |
13560 psi @Strain 0.820 %, Temperature -4.00 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo.. |