Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 9.20 MPa @Strain 300 %, Thickness 2.00 mm |
1330 psi @Strain 300 %, Thickness 0.0787 in |
Type 1, 200 mm/min; Flow; DIN 53504 |
PolyOne OnFlex™ BIO 5370A-E0004 Thermoplastic Elastomer (TPE) OnFlex™-Bio 5300 series thermoplastic elastomer compounds are soft thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% of renewable materi.. |
|||
Tensile Stress | 9.20 MPa @Strain 47.92 %, Temperature 100 °C |
1330 psi @Strain 47.92 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.20 MPa @Strain 45.0 %, Temperature 80.0 °C |
1330 psi @Strain 45.0 %, Temperature 176 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® DYM350BK TPC-ET+PBT
(Unverified Data**) Medium Modulus Polyester Elastomer with Excellent Impact Resistance Developed for Air Bag Door ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.20 MPa @Strain 195.71 %, Temperature 120 °C |
1330 psi @Strain 195.71 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 9.20 MPa @Strain 128.33 %, Temperature 150 °C |
1330 psi @Strain 128.33 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8441 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |