Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 81.4 MPa @Strain 10.4 %, Temperature -20.0 °C |
11800 psi @Strain 10.4 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |