Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.47 MPa @Strain 174.29 %, Temperature 90.0 °C |
1230 psi @Strain 174.29 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.47 MPa @Strain 71.79 %, Temperature 100 °C |
1230 psi @Strain 71.79 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.47 MPa @Strain 60.24 %, Temperature 120 °C |
1230 psi @Strain 60.24 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.47 MPa @Strain 0.230 %, Temperature 150 °C |
1230 psi @Strain 0.230 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin.. |