Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 78.9 MPa @Strain 5.60 %, Temperature 0.000 °C |
11400 psi @Strain 5.60 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved Processing Delrin 900P is a low viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical proper.. |
|||
Tensile Stress | 78.9 MPa @Strain 5.60 %, Temperature 0.000 °C |
11400 psi @Strain 5.60 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG900P is a low viscosity acetal homopolymer with improved thermal stability. It has been developed for consideration .. |
|||
Tensile Stress | 78.9 MPa @Strain 17.0 %, Temperature 0.000 °C |
11400 psi @Strain 17.0 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Tensile Stress | 78.9 MPa @Strain 2.17 %, Temperature 23.0 °C |
11400 psi @Strain 2.17 %, Temperature 73.4 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |