Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 78.0 MPa @Strain 4.00 % |
11300 psi @Strain 4.00 % |
|
Solvay TECHNYL® A 402H1 Natural PA66, DRY Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The .. |
|||
Tensile Stress | 78.0 MPa @Strain 4.00 % |
11300 psi @Strain 4.00 % |
|
Solvay TECHNYL® B 50 H1 PA66/6, DRY Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av.. |
|||
Tensile Stress | 78.0 MPa @Strain 5.00 %, Temperature 80.0 °C |
11300 psi @Strain 5.00 %, Temperature 176 °F |
|
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, Conditioned Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co.. |
|||
Tensile Stress | 78.0 MPa @Strain 4.00 %, Temperature 23.0 °C |
11300 psi @Strain 4.00 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan.. |
|||
Tensile Stress | 78.0 MPa @Strain 3.00 % |
11300 psi @Strain 3.00 % |
|
Solvay TECHNYL® A 218 PA66, 33% glass fiber, DRY Standard viscosity, heat stabilized for injection molding. It is available in natural and black colors.Benefits: This product offers all the primary properties of unreinforced polyamide 66. In addit.. |