Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 77.2 MPa @Strain 9.60 %, Temperature -40.0 °C |
11200 psi @Strain 9.60 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |