Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 76.5 MPa @Strain 9.00 %, Temperature 0.000 °C |
11100 psi @Strain 9.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |