Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 76.42 MPa @Strain 1.31 %, Temperature 23.0 °C |
11080 psi @Strain 1.31 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin with outstanding impact resistance developed usin.. |