Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 72.11 MPa @Strain 2.07 %, Temperature 23.0 °C |
10460 psi @Strain 2.07 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |