Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.83 MPa @Strain 103.46 %, Temperature 150 °C |
1140 psi @Strain 103.46 %, Temperature 302 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8163HVBK Polyester Elastomer TPC-ET
(Unverified Data**) 65 Shore D Polyester Elastomer with Heat Ageing Protection Developed for ExtrusionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.83 MPa @Strain 142.91 %, Temperature 120 °C |
1140 psi @Strain 142.91 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |