Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.65 MPa @Strain 300 %, Temperature 23.0 °C |
1110 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ FFC 2882-87 Thermoplastic Elastomer (TPE) Versaflex™ FFC 2882-87 is designed to pass several fatty food extraction conditions identified in EU Directive 2002/72/EC, FDA 21 CFR 177.2600, and GB 4806.1-94. Versaflex™ FFC 2882-87 will also o.. |
|||
Tensile Stress | 7.65 MPa @Strain 300 % |
1110 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® F7880 TPE, Fire Retardant Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Auto PartsSealsWire & Cable ElectronicsInformation from Alliance Polymers & Services, Distributor of Nantong Elastome.. |
|||
Tensile Stress | 7.65 MPa @Strain 17.27 %, Temperature 120 °C |
1110 psi @Strain 17.27 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.65 MPa @Strain 6.74 %, Temperature 120 °C |
1110 psi @Strain 6.74 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |