Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.64 MPa @Strain 130.69 %, Temperature 120 °C |
1110 psi @Strain 130.69 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.64 MPa @Strain 17.13 %, Temperature 120 °C |
1110 psi @Strain 17.13 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 7.64 MPa @Strain 4.83 %, Temperature 150 °C |
1110 psi @Strain 4.83 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien.. |