Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 7.58 MPa @Strain 100 % |
1100 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® F02-074B-8 TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |
|||
Tensile Stress | 7.58 MPa @Strain 300 % |
1100 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® F02-139A TPE, Halogen Free Extrusion Grade Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to.. |
|||
Tensile Stress | 7.58 MPa @Strain 300 % |
1100 psi @Strain 300 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL 0135-33 Styrene Butadiene Block Copolymer (SBC) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||
Tensile Stress | 7.58 MPa @Strain 300 % |
1100 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P1890 TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 7.58 MPa @Strain 100 % |
1100 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Telcar® TL-97-T0207A-110 Thermoplastic Elastomer Uses: Automotive Applications; Industrial Cable Insulation Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed:.. |
|||
Tensile Stress | 7.58 MPa @Strain 4.35 %, Temperature 150 °C |
1100 psi @Strain 4.35 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)
(Unverified Data**) Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also.. |
|||
Tensile Stress | 7.58 MPa @Strain 300 % |
1100 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 7.58 MPa @Strain 100 % |
1100 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P90A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P90A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 7.58 MPa @Strain 100 % |
1100 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P90A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P90A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 7.58 MPa @Strain 300 % |
1100 psi @Strain 300 % |
ISO 37 |
Alliance Polymers Viprene™ P85A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P85A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |