Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 64.57 MPa @Strain 0.683319 %, Temperature 23.0 °C |
9365 psi @Strain 0.683319 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |