Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 6.82 MPa @Strain 0.250 %, Temperature 150 °C |
989 psi @Strain 0.250 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS 32CG20HSL BK409 Nylon 610
(Unverified Data**) 20% Carbon/Glass Reinforced Renewably Sourced Polyamide 610 Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 6.82 MPa @Strain 0.250 %, Temperature 0.000 °C |
989 psi @Strain 0.250 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC3090 NC010 Nylon 610
(Unverified Data**) Unreinforced Renewably Sourced High Viscosity Polyamide 610 Developed for Extrusion Zytel RS LC3090 NC010 is a renewable sourced polyamide 610 containing a miniumu of 60% renewably sourced ingredien.. |