Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 6.00 MPa @Strain 300 % |
870 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S EF 80A-3S1977 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Tensile Stress | 6.00 MPa @Strain 10.0 % |
870 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® PB420-B TPC-ET Blow Molding Grade |
|||
Tensile Stress | 6.00 MPa @Strain 1.60 %, Temperature 150 °C |
870 psi @Strain 1.60 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by .. |
|||
Tensile Stress | 6.00 MPa @Strain 300 % |
870 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 5070A Thermoplastic Polyurethane Elastomer Zythane™ 5070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 6.00 MPa @Strain 100 % |
870 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 5090A Thermoplastic Polyurethane Elastomer Zythane™ 5090A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 6.00 MPa @Strain 300 % |
870 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 7070A Thermoplastic Polyurethane Elastomer Zythane™ 7070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 6.00 MPa @Strain 100 % |
870 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 7085A Thermoplastic Polyurethane Elastomer Zythane™ 7085A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 6.00 MPa @Strain 300 % |
870 psi @Strain 300 % |
|
AorTech Biomaterials Elast-Eon™ E5-130 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Tensile Stress | >= 6.00 MPa @Strain 300 % |
>= 870 psi @Strain 300 % |
ISO 37 |
Austin Novel Materials Texalan® 470A Polyester-based TPU Description: Can be considered as custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech |
|||
Tensile Stress | >= 6.00 MPa @Strain 100 % |
>= 870 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 585A Polyether-based TPU Description: Good low temperature resistance, hydro resistance, which can be used in cold and humid temperaturesInformation from Dawnentech |
|||
Tensile Stress | 6.00 MPa @Strain 300 % |
870 psi @Strain 300 % |
|
AorTech Biomaterials Elast-Eon™ E5-130 Biomedical Polyurethane Pellets Elast-Eon™ polymers are used in biomedical applications. They have high biostability so they can be used for long term implantation. |
|||
Tensile Stress | 6.00 MPa @Strain 10.0 % |
870 psi @Strain 10.0 % |
ISO 527-1/-2 |
DSM Arnitel® EB464-01 TPC-ET Antisqueak Blow Molding Grade |
|||
Tensile Stress | 6.00 MPa @Strain 50.0 % |
870 psi @Strain 50.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® G3548 NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 35 Shore D Standard Performance Polyester Elastomer with Non-discoloring StabilizerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 6.00 MPa @Strain 300 % |
870 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 4070A Thermoplastic Polyurethane Elastomer Zythane™ 4070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 6.00 MPa @Strain 100 % |
870 psi @Strain 100 % |
ASTM D412 |
Alliance Polymers Zythane™ 7085AU Thermoplastic Polyurethane Elastomer Zythane™ 7085UF is a UV stabilized polyether-based TPU specifically formulated for extrusion applications. It exhibits excellent abrasion resistance and toughness and has good hydrolytic stability,.. |