Polymer Property : Tensile Stress = 54.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 54.3 MPa

@Strain 2.60 %,
Temperature 23.0 °C
7880 psi

@Strain 2.60 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)  (Unverified Data**)
Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low..
Tensile Stress 54.3 MPa

@Strain 3.92 %,
Temperature 0.000 °C
7880 psi

@Strain 3.92 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide ..