Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 54.1 MPa @Strain 1.50 %, Temperature 90.0 °C |
7850 psi @Strain 1.50 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |