Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 53.92 MPa @Strain 7.92 %, Temperature 0.000 °C |
7820 psi @Strain 7.92 %, Temperature 32.0 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 53.92 MPa @Strain 0.500 %, Temperature -40.0 °C |
7820 psi @Strain 0.500 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 10B40 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B40 NC010 is a 40% mineral reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |