Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 50.93 MPa @Strain 17.77 %, Temperature 23.0 °C |
7387 psi @Strain 17.77 %, Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 50.93 MPa @Strain 1.01 %, Temperature 90.0 °C |
7387 psi @Strain 1.01 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSRX BK099 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSRX BK099 a 35% glass reinforced heat stabilized hydrolysis resistant PA66 for injection molding. Developed for applications designed fo.. |